ITEM
|
低端玻璃透镜
Low-end glass lens
|
高端光学玻璃透镜
High-end optical glass lens from KINGLUX
|
加工工艺Processing Technology
|
①无退火工序,透镜应力弱,防爆性能弱,易碎
No annealing step ,lens stress weak , explosion-proof performance is weak , fragile
|
①经过保温带工艺退火,透镜应力强,防爆性能好,不易摔碎
After annealing process , the lens would be strong,good explosion-proof performance, and not fragile
|
②工序,模压-粗磨-倒边-抛光,所有工序均为一出多,产品精度低,一致性差
Process: molding - roughing - bevelling - polished , all the processes are more than one , precision products is low, poor consistency
|
②工序,原材料抛光-模压-退火-敲边-粗磨-倒边-精磨-抛光-超声波清洗,所有工序均为一出一,保证产品精度以及一致性
Process: polishing materials - molded - annealing - Knock side - roughing - bevelling - grinding - polishing - ultrasonic cleaning , all the processes ensure product accuracy and consistency
|
②普通模具材料,模压成型透镜表面精度低
Common mold material lens is of low surface accuracy
|
③透镜模具采用日本进口特殊模具材料,模压成型的透镜表面精密度
高Japan imported special lens mold material ensure lens high surface accuracy
|
原材料选择Raw material selection
|
普通低价高硼硅3.3棒料,气泡,杂质,黑点,水纹等瑕疵多Common low-cost high borosilicate 3.3 bar , bubbles/ inclusions /black spots/waterlines and other defects more
|
采用高端特级精品高硼硅玻璃3.3棒料,透光率高,无气泡,杂质,黑点,水纹等瑕疵
Using premium quality borosilicate glass 3.3 bar , high transmittance, no bubbles /impurities/ black spots/ waterlines and other defects
|
表面品质Surface Quality
|
表面光泽度低,透镜穿透率低
Low surface glossiness , low penetration rate
|
表面光泽度高,透镜穿透率强
surface high glossiness, high penetration rate, low light loss
|
透光率light transmittance
|
80%~85%
|
90%~94%
|
防爆性能Proof performance
|
低low
|
高high
|
光型Light type
|
照度不均匀,黄斑严重,LED光效利用率
低Uneven illumination , macular serious , low efficiency utilization rate for LED
|
照明区域内照度均匀,能量高,提高LED的光效利用率Lighting illumination uniformity within the region , high energy, improve LED utilization efficiency
|